Flattening in a measurement curve can have different causes. Mainly, defects such as rot or fungal attack reduce the drilling resistance, which leads to a flattening of the curve. Another possible cause is tangential drilling. In this case, the drilling is not radial through the wood core but angled along the growth rings. The drill needle meets the tree rings at an angle significantly less than 90°. The standard procedure, in which drilling is done toward the wood center, is called radial drilling.
Tangential drilling causes flattening in the measurement curve because the needle no longer cuts perpendicularly through the hard latewood zones. The more the drilling deviates from the radial direction, the longer the needle can remain in a single zone, often the softer earlywood, which makes the flattening in the curve last longer. At the same time, individual tree rings in the measurement curve are less distinct or no longer recognizable.
A basic understanding of the growth ring structure of coniferous and deciduous trees is essential for interpretation:
- Conifers are known for their regular structure and clearly defined tree rings. The rings can be easily distinguished due to the marked transition from light earlywood to dark latewood. The wood structure is relatively uniform and consists mostly of tracheids.
- Deciduous trees, on the other hand, have a more complex structure that varies depending on the species. Some species, such as oak or ash, are called “ring-porous.” These trees form large pores in the earlywood, visible as a light, wide ring, followed by denser latewood. This results in distinct and clearly visible amplitudes in the curve.
- Other deciduous trees, such as beech or birch, are “diffuse-porous.” Here, the pores are distributed throughout the ring, making growth rings harder to recognize and less contrasted. This is reflected in the measurement curve: a clear tree ring structure is not always visible in these species.
Geography also plays a role. In tropical regions without pronounced seasons, trees often form no or only weakly defined tree rings.
Conclusion: Flattening is not necessarily caused by a defect. Interpretation depends on the wood species and drilling angle. If flattening occurs, several factors should be checked, including the course of the drilling.
Checklist for your measurement:
- Position the drill as perpendicular as possible to the tree rings.
- Always use a sharp drill needle to prevent deflection.
- Keep the device steady during drilling to avoid changing the angle.